ASD-STAN prEN 2811

Nuts, hexagon, slotted/castellated in steel cadmium plated – Classification : 1100 MPa/235 deg C
Data Sheet by ASD-STAN Standardization, 02/16/1987

ASD-STAN prEN 2763

Steel FE-PL1504 (33CrMoV12) Air Melted Hardened and Tempered Bar for Machining De <or= 80 mm 1 200 MPa <or= Rm <or= 1 350 Mpa
Data Sheet by ASD-STAN Standardization, 12/31/1998

ASD-STAN prEN 3988

Test methods for metallic materials – Constant amplitude strain-controlled low cycle fatigue testing
Data Sheet by ASD-STAN Standardization, 04/30/1998

ASD-STAN prEN 4268

Aerospace series – Metallic materials – Heat treatment facilities – General requirements
Data Sheet by ASD-STAN Standardization, 09/01/2010

ASD-STAN prEN 9300-010

Aerospace series – LOTAR LOng Term Archiving and Retrieval of digital technical product documentation such as 3D, CAD and PDM data – Part 010: Overview Data Flow
Data Sheet by ASD-STAN Standardization, 10/31/2006

ASD-STAN prEN 6126

Aerospace series – Fitting end, 24deg internal cone, external thread, flareless type, size -32 – Tube diameter D = 2 inches (D = 50,8 mm) – Extra fine thread pitch – Inch series – Design standard
Data Sheet by ASD-STAN Standardization, 01/31/2005

ASD-STAN prEN 2712-004

Cables, electrical, single and multicore for general purpose – Operating temperatures between -55 deg C and 150 deg C – Part 004: Screened (braided) and jacketed, ink jet printable – Product standard
Data Sheet by ASD-STAN Standardization, 03/31/1995

ASD-STAN prEN 2591-214

Aerospace series – elements of electrical and optical connection – Test methods – Part 214 :Lightning strike, current and voltage pulse
Data Sheet by ASD-STAN Standardization, 02/28/2011

ASD-STAN prEN 4612-012

Aerospace series – Cables, electrical, for general purpose, single and multicore assembly XLETFE Family jacketed or screened and jacketed – Part 012: Nickel plated copper – Operating temperatures, between – 65 deg C and 150 deg C – Dual extruded wall for open a
Data Sheet by ASD-STAN Standardization, 03/31/2005